I wanted to solder up the core plugs top and bottom of my king pins and was recommended Bakers No 3 soldering fluid. Absolute cleanliness and this stuff seemed to help the solder flow very well. Prior to that I had managed the usual amateur's trick of blobs of solder everywhere except where you want it. It is corrosive so you need to wash off any excess.
P.S. Thanks to Derek in the following post for pointing that out. I had the wrong end of stick I'm afraid.