I am glad I did not broach the topic but just in case anyone makes wrong assumptions, on 1934 and Girling stubs I have found them cracked at the large radius. On my car half thru the tube at 100,000 lhs, rhs ok. A mate had one shear off, fortunately at 1/2 mph when pushing the car! Cars here had a hard life with a lot of metal road corrugations and broken road edges.
(incidentally, on other makes of cars and on trailers cornered hard failure often occurs from the top side)
If testers here twig that welding or heating has been applied it is or is supposed to be a w.o.f fail.
(incidentally, on other makes of cars and on trailers cornered hard failure often occurs from the top side)